Soldering of solution-processed organic vertical transistor and light-emitting diode on separate glass substrates by tin micro-balls

Yu Hsin Lin, Yu Fan Chang, Hsin-Fei Meng*, Hsiao-Wen Zan, Wen-Syang Hsu, Chao Hsuan Chen

*此作品的通信作者

研究成果: Article同行評審

4 引文 斯高帕斯(Scopus)

摘要

The vertical organic space-charge-limited transistor made of P3HT and small-molecule phosphorescent organic light-emitting diode (OLED) are made on two separate glass substrate by blade coating, then soldered vertically together by tin balls with 40 μm diameter. The soldering is done by hot wind of 150 C for 5 min Contact resistance is only 10 Ω. The vertical transistor is annealed at 150 C for 5 min before soldering to enhance the output current up to 25 mA/cm2 and give high thermal stability. Both OLED and the annealed vertical transistor are not affected by the soldering process. The vertical transistor has 1/4 of the OLED area and turns on the bottom-emission white OLED up to 300 cd/m2 and orange OLED up to 600 cd/m 2. The entire operation is within 8 V. OLED and transistor array can therefore be made on separate glass substrates then soldered together to form the display.

原文English
頁(從 - 到)3052-3060
頁數9
期刊Organic Electronics
14
發行號11
DOIs
出版狀態Published - 2013

指紋

深入研究「Soldering of solution-processed organic vertical transistor and light-emitting diode on separate glass substrates by tin micro-balls」主題。共同形成了獨特的指紋。

引用此